Monel K500, N05500, 2.4375, Nickel Alloy Spring Wire

Ask Latest Price
Video Channel
Brand Name :fushun
Model Number :K500
Certification :ISO NQA
Place of Origin :CHINA
MOQ :1KG
Payment Terms :L/C, T/T, D/P, D/A
Delivery Time :1
Material :Nickel Alloy
Application :Spring
Contact Now

Add to Cart

Find Similar Videos
View Product Description

Monel K500, N05500, 2.4375, Nickel Alloy Spring Wire

This Nickel-Copper alloy is precipitation hardenable, due to the additions of Aluminium and Titanium. It combines the corrosion resistance of Monel 400 but gives the added advantage of extra strength and hardness (as a result of its age hardening ability). Monel K500 provides corrosion resistance in several marine and chemical applications.

Monel K500 is also known as Nicorros Al.

Size

Diameter: 0.1 - 40mm

Shape: round, square, flat, special shaped

Key Features

  • Corrosion resistance similar to Monel 400 but with higher strength and hardness.
  • Low permeability and is non-magnetic to temperatures as low as -101°C (-150°F).
  • Age hardenable.
  • Good for sea water applications.

Typical Applications

Pump Shafts

Fasteners

Marine Propeller Shafts

Oil Well Tools

Instruments

Springs

Designations

W.Nr 2.4375

UNS N05500

AWS 041

Specifications

ASTM B865

BS 3075 NA 18

BS 3076 NA 18

ISO 15156-3

(NACE MR 0175)

QQ-N-286

Chemical Composition

Element Min % Max %
Ni 63 70
Co 2
Cu 27 33
Fe 2
Al 2.3 3.2
C 0.25
Si 1
Mn 1.5
Ti 0.35 0.85
S 0.01

Physical Properties

Density Melting Point Coefficient of Expansion Modulus of Rigidity Modulus of Elasticity
8.44 g/cm³ 1350 °C Coefficient of Expansion
13.7 μm/m °C (20 – 100 °C)
66 kN/mm² 179 kN/mm²
0.305 lb/in³ 2460 °F 7.6 x 10-6 in/in °F (70 – 212 °F) 9573 ksi 25962 ksi

Heat treatment

Condition Type Temperature Time Cooling
Annealed Age Harden 580 – 590 °C (1075 – 1095 °F) 8 – 10 Hr Air
Spring Temper Age Harden 530 – 540 °C (985 – 1005 °F) 4 – 6 Hr Air

Mechanical Properties

Annealed Approx. tensile strength <850 N/mm² <123 ksi
Approx. operating temperature -100 to +260 °C -150 to +500 °F
Annealed + Aged Approx. tensile strength >950 N/mm² >138 ksi
Approx. operating temperature -100 to +260 °C -150 to +500 °F
Spring Temper Approx. tensile strength 1000 – 1300 N/mm² 145 – 189 ksi
Approx. operating temperature -100 to +260 °C -150 to +500 °F
Spring Temper + Aged Approx. tensile strength 1200 – 1500 N/mm² 174 – 218 ksi
Approx. operating temperature -100 to +260 °C -150 to +500 °F