Hunan Fushun Metal Co., Ltd.

Hunan Fushun Metal Co., Ltd.

Manufacturer from China
Site Member
4 Years
Home / Products / Nickel Spring Wire /

Waspaloy, 2.4654, N07001, Nickel Alloy Spring Wire

Contact Now
Hunan Fushun Metal Co., Ltd.
City:changsha
Province/State:hunan
Country/Region:china
Contact Person:MsFlorence Tang
Contact Now

Waspaloy, 2.4654, N07001, Nickel Alloy Spring Wire

Ask Latest Price
Video Channel
Brand Name :fushun
Model Number :2.4654
Certification :ISO NQA
Place of Origin :CHINA
MOQ :1KG
Payment Terms :L/C, T/T, D/P, D/A
Delivery Time :1
Material :Nickel Alloy
Application :Spring
Contact Now

Add to Cart

Find Similar Videos
View Product Description

Waspaloy, 2.4654, N07001, Nickel Alloy Spring Wire

This age hardenable nickel base super alloy has very good strength in temperatures up to about 980°C (1800°F). It’s strength is generally comparable to that of Rene 41 and is generally superior to that of Alloy 718 at temperatures exceeding 650 – 705°C (1200 – 1300°F).

Size

Diameter: 0.1 - 40mm

Shape: round, square, flat, special shaped

Key Features

  • Very high strength at elevated temperatures.
  • Strength is generally comparable to that of Rene 41 and generally superior to Inconel 718.
  • Age hardenable.
  • High temperature dynamic applications.

Typical Applications

Gas turbine engine parts

Aerospace components

Springs and fasteners

Designations

W.Nr 2.4654

UNS N07001

AWS 170

Specifications

AMS 5544

AMS 5706

AMS 5708

AMS 5828

ASTM B637

Chemical Composition

Element Min % Max %
C 0.02 0.1
Mn 0.1
Si 0.1
P 0.01
S 0.01
Cr 18 21
Co 12 15
Mo 3.5 5
Ti 2.75 3.5
Al 1.2 1.6
B 0.003 0.01
Zr 0.04
Fe 2
Cu 0.1
Ni bal bal

Physical Properties

Density Melting Point Coefficient of Expansion Modulus of Rigidity Modulus of Elasticity
8.16 g/cm³ 1330 °C 12.2 μm/m °C (20 – 100 °C) 81 kN/mm² 211.0 kN/mm²
0.295 lb/in³ 2425 °F 6.8 x 10-6 in/in °F (70 – 212 °F) 11750 ksi 30600 ksi

Heat treatment

Condition Type Temperature Time Cooling
Annealed Stabilize
Age Harden
843 °C (1550 °F)
760 °C (1400 °F)
4 Hr
16 Hr
Air
Air
Spring Temper Anneal
Stabilize
Age Harden
1050 °C (1920 °F)
843 °C (1550 °F)
760 °C (1400 °F)
4 Hr
4 Hr
16 Hr
Air
Air
Air

Mechanical Properties

Solution Annealed Approx. tensile strength <1100 N/mm² <159 ksi
Approx. operating temperature depending on load and environment
Solution Annealed + Aged Approx. tensile strength 1300 – 1500 N/mm² 189 – 218 ksi
Approx. operating temperature depending on load and environment up to +550 °C up to +1020 °F
Spring Temper Approx. tensile strength 1300 – 1600 N/mm² 189 – 232 ksi
Approx. operating temperature depending on load and environment
Spring Temper + Annealed + Aged Approx. tensile strength 1300 – 1500 N/mm² 189 – 218 ksi
Approx. operating temperature depending on load and environment up to +550 °C up to +1020 °F