Hunan Fushun Metal Co., Ltd.

Hunan Fushun Metal Co., Ltd.

Manufacturer from China
Site Member
4 Years
Home / Products / Nickel Spring Wire /

Haynes 282, N07208, Nickel Alloy Spring Wire

Contact Now
Hunan Fushun Metal Co., Ltd.
City:changsha
Province/State:hunan
Country/Region:china
Contact Person:MsFlorence Tang
Contact Now

Haynes 282, N07208, Nickel Alloy Spring Wire

Ask Latest Price
Video Channel
Brand Name :fushun
Model Number :282
Certification :ISO NQA
Place of Origin :CHINA
MOQ :1KG
Payment Terms :L/C, T/T, D/P, D/A
Delivery Time :1
Material :Nickel Alloy
Application :Spring
Contact Now

Add to Cart

Find Similar Videos
View Product Description

Haynes 282, N07208, Nickel Alloy Spring Wire

Haynes 282 is a new alloy developed for high temperature structural applications which has excellent creep strength in the temperature range of 650 – 930 °C (1200 – 1700 °F), surpassing that of Waspalloy and Rene 41. Haynes 282 possesses a unique combination of creep strength, thermal stability, weldability and fabricability that is not found in currently available commercial alloys. Its features make it suitable for critical gas turbine applications such as combustors, turbine and exhaust sections, and nozzle components.

Key Features

New alloy developed for high temperature structural applications which has excellent creep strength in the temperature range of 650 – 930 °C (1200 – 1700 °F), surpassing that of Waspalloy and Rene 41.

Excellent creep strength.

Typical Applications

Exhaust nozzle components in augmented aircraft gas turbines, hot gas paths in land based gas turbines.

A potential choice for high temperature development parts.

High temperature static applications.

Designations

UNS N07208

AWS 062

Chemical Composition

Element Min % Max %
Al 1.38 1.65
B 0.003 0.01
C 0.04 0.08
Nb 0.2
Co 9 11
Cr 18.5 20.5
Cu 0.1
Fe 1.5
Mn 0.3
Mo 8 9
Ni bal
P 0.015
S 0.015
Si 0.15
Ta 0.1
Ti 1.9 2.3
W 0.5

Physical Properties

Density Melting Point Coefficient of Expansion
8.27 g/cm³ 1300 – 1375 °C 12.1 μm/m °C (20 – 100 °C)
0.3 lb/in³ 2370 – 2510 °F 6.7 x 10-6 in/in °F (70 – 212 °F)

Heat treatment

Condition Type Temperature Time Cooling
Spring Temper Stablise 1010 °C (1850 °F) 2 Hr Air
Spring Temper Age Harden 790 °C (1450 °F) 8 Hr Air

Mechanical Properties

Annealed Approx. tensile strength 800 – 1200 N/mm² 116 – 174 ksi
Approx. operating temperature depending on load** and environment Contact Alloy Wire for information Contact Alloy Wire for information
Spring Temper Approx. tensile strength 1300 – 1600 N/mm² 190 – 232 ksi
Approx. operating temperature depending on load** and environment Contact Alloy Wire for information Contact Alloy Wire for information
Spring Temper + Stabilised and Aged Approx. tensile strength 1000 – 1300 N/mm² 145 – 190 ksi
Approx. operating temperature depending on load** and environment Contact Alloy Wire for information Contact Alloy Wire for information