Hastelloy C22, 2.4602, N06022, Nickel Alloy Spring Wire

Ask Latest Price
Video Channel
Brand Name :fushun
Model Number :C22
Certification :ISO NQA
Place of Origin :CHINA
MOQ :1KG
Payment Terms :L/C, T/T, D/P, D/A
Delivery Time :1
Material :Nickel Alloy
Application :Spring
Contact Now

Add to Cart

Find Similar Videos
View Product Description

Hastelloy C22, 2.4602, N06022, Nickel Alloy Spring Wire

A Nickel-Chromium-Molybdenum alloy with better overall resistance and versatility than any other NiCrMo available. It has excellent resistance to localised corrosion and to a variety of mixed industrial chemicals. Hastelloy C22 is used in severely corrosive media involving high chloride and temperature applications such as buffer solutions, active pharmaceutical ingredients (API), fabric softeners, cleaning supplies, and condiments such as soy and chili sauce. Like other nickel alloys, Hastelloy C22 is extremely ductile, exhibits exceptional weldability, and can easily be fabricated into industrial components.

Hastelloy C22 is also known as Nicrofer 5621, Superimphy C22, and Inconel 622.

Size

Diameter: 0.1 - 40mm

Shape: round, square, flat, special shaped

Key Features

Hastelloy C22 offers the following key features:

Better overall corrosion resistance than Hastelloy C-4 & C-276 and Inconel 625.

Outstanding resistance to pitting, crevice corrosion and stress corrosion cracking.

Typical Applications

Hastelloy C22 is known to be suitable for the following applications:

Chlorination systems

Nuclear fuel reprocessing

Pickling systems

Designations

W.Nr 2.4602

UNS N06022

AWS 053

Specifications

ASTM B574

ASTM B575

ASTM B619

ISO 15156-3 (NACE MR 0175)

Chemical Composition

Element Min % Max %
Cr 20 22.5
Mo 12.5 14.5
Fe 2 6
W 2.5 3.5
C 0.015
Si 0.08
Co 2.5
Mn 0.5
V 0.35
P 0.02
S 0.02
Ni Bal

Physical Properties

Density Melting Point Coefficient of Expansion Modulus of Rigidity Modulus of Elasticity
8.69 g/cm³ 1399 °C 12.4 μm/m °C (20 – 100 °C) 78.6 kN/mm² 205.5 kN/mm²
0.314 lb/in³ 2550 °F 6.9 x 10-6 in/in °F (70 – 212 °F) 11400 ksi 29806 ksi

Heat treatment

Condition Type Temperature Time Cooling
Annealed or Spring Temper Stress Relieve 400 – 450 °C (750 – 840 °F) 2 Hr Air

Mechanical Properties

Annealed Approx. tensile strength <1100 N/mm² <159 ksi
Approx. operating temperature depending on load** and environment -200 to +400 °C -330 to +750 °F
Spring Temper Approx. tensile strength 1400 – 1700 N/mm² 203 – 247 ksi
Approx. operating temperature depending on load** and environment -200 to +400 °C -330 to +750 °F